With the widespread expansion of titanium applications and its significant increase in usage, the issue of recycling titanium resources after consumption has emerged. Focusing on titanium alloys with high usage, such as TC4 (Ti-6Al-4V), this article proposes a titanium separation and recovery method based on molten salt electrolysis.
The processing of titanium magnetite ores usually entails a combination of magnetic separation, gravity enrichment, flotation, and a comprehensive technique that includes preparatory roasting [[10], [11], [12]].This intricate procedure …
Keywords: extraction, titanium, separation, D2EHP A, PC-88A and stripping. INTRODUCTION. Titanium metal has become known as a space-age metal because of its high stren-
kiln pre-reduction-electric furnace method to treat vanadium-titanium magnetite, separated iron, vanadium and titanium efficiently, and enriched titanium into slag efficiently [24–26]. It can be observed that, whether it is the separation of raw ore or the use of metallurgical
Titanium extraction. The overall process. Titanium is extracted from its ore, rutile - TiO 2. It is first converted into titanium(IV) chloride, which is then reduced to titanium using either magnesium or sodium. Conversion of TiO 2 into TiCl 4. The ore rutile (impure titanium(IV) oxide) is heated with chlorine and coke at a temperature of about ...
Efficient separation of scandium and titanium is the premise for the recovery of these two valuable metals from red mud. In order to achieve the effective separation and selective recovery of scandium and titanium, in this work, we proposed a neutralization precipitation-acid leaching method based on the difference between the hydrolysis ...
In this study, a novel approach for the separation and recovery of titanium, scandium, and iron from acidic wastewater and red gypsum utilization has been investigated. …
In the separation of raw ore, Zhang Yanhua and Han Yuexin et al. used weak magnetics to enrich vanadium-titanium magnetite with strong magnetism, and then selected gravity separation, high gradient magnetic separation, electric separation, flotation or their combined processes to obtain titanium concentrate products according to the differences ...
The subsequent separation of scandium and titanium from the scandium-titanium residue is the key to recover these two valuable metals from the red mud. Based on the difference in hydrolysis behavior between titanium and scandium, it is feasible to keep the titanium remaining in the solid phase while gradually leaching the scandium species to ...
The separation and recovery of scandium and titanium from hydrolyzed sulfuric acid solution of titanium dioxide production using solvent extraction was investigated. A mixed solution of Na 3 PO 4 and H 2 O 2 was used to selectively scrub titanium from the loaded organic solution containing scandium and titanium.
The extraction and separation of titanium and iron from a simulated titanium dioxide solution by sulfuric acid method was systematically studied using TRPO as the extractant. The results showed that by appropriately adjusting the concentration of titanium solution and organic phase composition, the single-stage extraction rate of titanium could ...
The separation of titanium (Ti) (IV) in acidic leach solutions of vanadium slag by solvent extraction with ctyl tertiary amine (N235) is proposed. Because the leach solutions contain a lot of vanadium (V) and iron (Fe) impurities, the effects of various conditions on the separation of Ti, V, and Fe were investigated. Then, the extraction ...
The dumping of a large amount of steel slag not only wastes metal resources, but pollutes the ecological environment. In this study, a method for recovery of vanadium, titanium, iron, magnesium, and synthesizing anhydrite from steel slag is proposed. The leaching efficiency of V, Ti, Fe, and Mg was 99.42%, 99.36%, 99.89%, and 99.95%, respectively, under a H2SO4 …
To develop a flowsheet for separation of high grade titanium-rutile from ilmenite, that will meet market requirements. Rutile has a SG of 4.2, hardness 6.0 to 6.5 and is non-magnetic; while ilmenite has a SG of 4.5 to 5.0, hardness of 5.0 to 6.0, and is weakly magnetic.
The separation of titanium (Ti) (IV) in acidic leach solutions of vanadium slag by solvent extraction with ctyl tertiary amine (N235) is proposed. Because the leach solutions contain a lot of ...
By controlling the hydrolysis rate of titanium alcohol, sufficient sites with adjustable defects for adsorption can be obtained, which may be useful for V(V)/Cr(VI) separation. In this work, amorphous-titanium-based microspheres (ATMs) are prepared by hydrolysis during coordination at room temperature.
In this study, a full process in recovery of titanium and rare earth elements (REEs) from the red mud was developed. The suggested route consists of four main stages in the process flow diagram: sample preparation, leaching, hydrolysis, and solvent extraction.Sample preparation is proposed using a two-stage water washing followed by calcination to remove …
Solvent extraction separation of titanium(IV), vanadium(V) and iron(III) from simulated waste chloride liquors of titanium minerals processing industry by the trialkylphosphine oxide Cyanex 923. P Narayanan Remya, P Narayanan Remya.
The vanadium–bearing titanomagnetite (VBT) is a strategic and complex iron ore, which containing valuable metals of vanadium, titanium, and iron used as constituents of several alloys, whitepigments, and steel [1], [2], [3].In China, the gross reserve of titanium in VBT ore is estimated to be about 1.18 million tons, accounting for 93% of China's total domestic reserve …
The separation of titanium, vanadium and chromium in vanadium slag (VS) is a difficult problem restricting the comprehensive utilization of VS. This paper presents the first study on the separation of titanium, vanadium and chromium from oxalic acid leachate of VS. Firstly, the separation of titanium from the leachate by hydrothermal method was ...
A method for the production of titanium metal from titanium-bearing ore. The method comprises leaching said ore or a concentrate thereof with an aqueous solution of a hydrogen halide; separating solids from the leach solution, to provide a leachate solution. The leachate solution may be subjected to extraction with an immiscible organic phase to selectively remove iron …
Titanium dioxide (TiO 2) is widely applied in thermal coating materials, semiconductors, plastic products, and chemical catalysts due to its remarkable physical–chemical properties [1], [2], [3], [4].In China, titanium resources are mainly distributed in the Panxi and Chengde areas [5], renowned for their diverse range, substantial reserves, and abundant distribution [6].
Vanadium titanomagnetite (VTM) is an important mineral for developing titanium resources, but the comprehensive recovery of ilmenite separation is extremely poor, resulting in the low-efficiency utilization of titanium resources. Here, the separation of ilmenite from VTM ore is studied by combining magnetic separation and flotation technologies. In particular, the …
The separation and extraction of titanium, iron, and alumina in one spot can shorten the process and make full use of the electric energy. Under optimal conditions, the efficiencies of iron, titanium, and alumina were 97.6%, 93.1% and 88.5%, respectively.
DOI: 10.1016/j.seppur.2020.117169 Corpus ID: 219743539; Efficient separation of vanadium, titanium, and iron from vanadium-bearing titanomagnetite by pressurized pyrolysis of ammonium chloride-acid leaching-solvent extraction process
The extraction of high-titanium titanium magnetite ores presents notable technological difficulties owing to many unique factors. Firstly, the ores consist of closely …
Therefore, titanium minerals and iron minerals can be easily separated via magnetic separation, and titanium and vanadium can be separated simultaneously. 4) The proposed magnetic roasting technology provides a new idea and method for the separation of vanadium and titanium from hematite containing vanadium and titanium, as well as the ...
In this paper, magnetization roasting - low-intensity magnetic separation was performed on a pre-concentration concentrate obtained from an Australian hematite containing titanium and vanadium to realize the separation of titanium and vanadium. The results showed that an iron concentrate with TFe (total iron) grade of 58.71%, iron recovery of 86.72% and V 2 …
Red mud discharged from alumina production is a valuable metal resource of great importance in the context of the requirement to reduce the impact of mining on the environment and resource consumption. The efficient dissolution of iron from red mud by oxalic acid has been reported. Although the concentrations of aluminum, silicon, and titanium were also high in the …
The separation retention time was held to be 5 min, after which the samples of effluent and floats were immediately obtained for the performance evaluation and TiO 2-NP fate analysis. The treated water (10 mL) was first collected from the bottom of the separation jar, noting that the initial 5 mL of effluent was discarded.
In this study, a process of Electrostatic Separation-Oxidative Roasting-Acid Leaching was applied to separate and recover titanium from TAGS. The results indicate that …